Murtfeldt Original Material ”S”® plus + FP Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Original Material ”S”®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Original Material ”S”® plus + FP Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “food protect” and embodies two vital properties: This product is both food-safe and metal-detectable.Special Properties:• Metal-detectable in all commonly used industrial detectors• Approved for use in the food industry (EU and FDA) • Very good wear and abrasion resistance• Extremely good machinability• Excellent chemical resistance• Increased continuous use temperature of 100°CInformation provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density <= 1.14 g/cc
<= 0.0412 lb/in³
ISO 1183
Molecular Weight 9.00e+6 g/mol
9.00e+6 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
DIN 53505
Ball Indentation Hardness 40.0 MPa
5800 psi
Tensile Strength 26.0 MPa
3770 psi
ISO 527
Elongation at Break 250 %
250 %
ISO 527
Modulus of Elasticity 0.700 GPa
102 ksi
Charpy Impact, Notched >= 10.0 J/cm²
>= 47.6 ft-lb/in²
ISO 179
Coefficient of Friction, Dynamic 0.10 - 0.20
0.10 - 0.20
Sand Slurry 100
100
value in %
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 23.0 - 60.0 °C
111 µin/in-°F

@Temperature 73.4 - 140 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
ISO 52612
Maximum Service Temperature, Air 120 °C
248 °F
Short Term
80.0 °C

@Time 1.80e+7 sec
176 °F

@Time 5000 hour
Minimum Service Temperature, Air -200 °C
-328 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity <= 1.00e+12 ohm-cm
<= 1.00e+12 ohm-cm
IEC 60093
Surface Resistance <= 1.00e+12 ohm
<= 1.00e+12 ohm
IEC 60093
Dielectric Strength <= 45.0 kV/mm
<= 1140 kV/in
IEC 60243
Compliance Properties Metric English Comments
European Food 1935/2004 Yes
Yes
FDA Yes
Yes
Descriptive Properties Value Comments
Color Light Blue