Mechanical Properties Metric English Comments
Charpy Impact, Notched >= 10.0 J/cm²
>= 47.6 ft-lb/in²
ISO 179
Murtfeldt Original Material ”S”® plus + FP Polyethylene
Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “..
Charpy Impact, Notched >= 10.0 J/cm²
>= 47.6 ft-lb/in²
ISO 179
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from ..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
Partial Break; ISO 179-1/1eA
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data)
Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
Partial Break; ISO 179-1/1eA
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data)
TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
Partial Break; ISO 179-1/1eA
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data)
TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
ISO 179
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP
SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
LATI Latamid 6 E02 PA 6, Impact modified
Polyamide 6 (PA6). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A...
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
ISO 179/1EA-1993
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 246M PA66, Conditioned
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
ISO Data
Styron CALIBREâ„¢ 200 4 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
ISO Data
Styron CALIBREâ„¢ 300 4 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
ISO Data
Dow Prevail® 3100 ABS + Polyurethane
PREVAIL® 3100 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used ..
Charpy Impact, Notched 10.0 J/cm²

@Temperature -20.0 °C
47.6 ft-lb/in²

@Temperature -4.00 °F
After conditioning at 23°C/50%RH; ISO 179/Af
Arkema Group Orgalloy® RS 6620 Polyamide 6.6 Alloy 20% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group
Charpy Impact, Notched >= 10.0 J/cm²
>= 47.6 ft-lb/in²
Determined with double-notched specimens; ISO 11542-2
Braskem UTEC® 5040 Ultra High Molecular Weight Polyethylene
Applications which require high wear resistance - technical parts, RAM extruded and compression molded sheets, rods and profiles.Information provided by Braskem.
Charpy Impact, Notched >= 10.0 J/cm²
>= 47.6 ft-lb/in²
Determined with double-notched specimens; ISO 11542-2
Braskem UTEC® 5041 Ultra High Molecular Weight Polyethylene
Applications which require high wear resistance and the use of pigments and/or additives - technical parts, RAM extruded and compression molded sheets, rods and profiles.Information provided by Bras..
Charpy Impact, Notched >= 10.0 J/cm²
>= 47.6 ft-lb/in²
Determined with double-notched specimens; ISO 11542-2
Braskem UTEC® 6540 Ultra High Molecular Weight Polyethylene
Applications which require highest wear resistance - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided by Braskem.
Charpy Impact, Notched >= 10.0 J/cm²
>= 47.6 ft-lb/in²
Determined with double-notched specimens; ISO 11542-2
Braskem UTEC® 6541 Ultra High Molecular Weight Polyethylene
Applications which require highest wear resistance and the use of pigments and/or additives - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided b..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
ISO 179
BASF Ultramid® 8350 HS PA6 (Dry)
Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® BRZ 334 H PA6
Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® L 25A NZ PA12-I
Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid..
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® L 25A NZ PA12-I
Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid..