Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 40.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 40.0 MPa
5800 psi
Murtfeldt Original Material ”S”® plus + FP Polyethylene
Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “..
Ball Indentation Hardness 40.0 MPa
5800 psi
ISO2039.1 DIN.53456
Omnia Plastica PE 1000 - Polyethylene 1000
Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is there..
Ball Indentation Hardness 40.0 MPa
5800 psi
ISO 2039-1
Quadrant EPP Cestilene™ HD 1000 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Ball Indentation Hardness 40.0 MPa
5800 psi
ISO 2039-1
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data)
This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica..
Ball Indentation Hardness 40.0 MPa
5800 psi
ISO 2039-1
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data)
Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg..
Ball Indentation Hardness 40.0 - 135 MPa
5800 - 19600 psi
Average value: 75.0 MPa Grade Count:5
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
Ball Indentation Hardness 40.0 MPa
5800 psi
ASTM 1457-62 T
Fluorseals PTFE 60% bronze filled
Improved compressive strength and thermal conductivity.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Ball Indentation Hardness 40.0 MPa
5800 psi
H385/30; ISO 2039
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed..
Ball Indentation Hardness 40.0 MPa
5800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BFZ 3 PA6
Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril..
Ball Indentation Hardness 40.0 MPa
5800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BZ 3 PA6
Information provided by EMS Grivory
Ball Indentation Hardness 40.0 MPa
5800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® EB 50 H DZ PA6
Product description: Grilon EB 50 H DZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon EB 50 H DZ has the following important properties:..
Ball Indentation Hardness 40.0 MPa
5800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® L 25 W 20 PA12
Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila..
Ball Indentation Hardness 40.0 MPa
5800 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-B40 PTFE
Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 40.0 - 44.0 MPa
5800 - 6380 psi
ISO 2032
Adamas Adalon® 826 PTFE, 50% Stainless steel
Information provided by Adamas, HPM
Ball Indentation Hardness 40.0 - 46.0 MPa
5800 - 6670 psi
ISO 2032-N132
Adamas Adalon® 503 PTFE, 0.1% MoS2
Information provided by Adamas, HPM
Ball Indentation Hardness 40.0 MPa
5800 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I
Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril..
Ball Indentation Hardness 40.0 MPa
5800 psi
value at 30 sec.; ISO 2039-1
CENTROPLAST CENTROLEN PE-UHMW Ultra-high molecular weight polyethylene
This plastic is a low density, easily machined material that can be welded and has a low sliding friction with high impact resistance. Applications include glide strips, pump components, and wearin..
Copyright © lookpolymers.com All Rights Reserved