Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955-89
Melt Flow 19 g/10 min
19 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.1 MPa
3210 psi
ASTM D638-95
Elongation at Break 125 %
125 %
ASTM D638-95
Flexural Strength 35.2 MPa
5110 psi
ASTM D790-95
Flexural Modulus 1.724 GPa
250.0 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256-93a
Gardner Impact 8.50 J
6.27 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648-95