Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | ASTM D638-95 |
Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | ASTM D638 |
DuPont™ Surlyn® 9970 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9970 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | |
Freudenberg Simrit Simriz® 484 FDA FFKT Perfluoroelastomer Compound Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of .. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | Cured |
KKPC Kumho RM 21L High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | |
Sylvin Technologies 9604-95 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | |
Williams Advanced Alloys WS96 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | ASTM D638 |
Total PPR 7425 Polypropylene, Injection Molding Grade Random copolymer for injection moldingClarity - FINA 7425, a random copolymer, exhibits excellent clarity when molded in polished molds.Impact - FINA 7425 produced molded parts with measurably impro.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE) Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | ASTM D638 |
DuPont™ Surlyn® 9650 Ionomer Resin, Zinc Surlyn® 9650 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | |
Dow AFFINITY™ VP 8770 Polyolefin Plastomer AFFINITY® VP 8770 polyolefin plastomer is an alpha-olefin resin for general purpose applications. It exhibits excellent optics and flexibility. Its low specific gravity can help control resin and p.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | Molded property |
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D412 |
Colorite Polymers CS1533UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D412 |
Colorite Polymers CS9034SR Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Colorite Polymers 9000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Colorite Polymers 9002 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Colorite Polymers 9077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Colorite Polymers 9813 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D412 |
Colorite Polymers CS1535UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | Bond strength to glass |
Dymax Light Weld® 426 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | ASTM D638 |
Buckeye Polymers BP PP 0015 R Blk Reprocessed Polypropylene, Unfilled PP Homo BlackThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compound.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | 2 in/min (50 mm/min); ASTM D638 |
Bapolene® PP5021 Polypropylene, Blow Molding Grade Bapolene PP5021 is a PP Random Copolymer designed for blow molding and extrusion applications. This resin exhibits excellent clarity, impact strength, stiffness and processability. This product me.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3200 psi | ASTM D638 |
Arkema Group Solarkote® P-600 Acrylic PVC Capstock, clear, high glossInformation provided by Arkema Group |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | ASTM D638 |
Buckeye Polymers BP Flex D7030 UC85 TPO Bumpers, Air damsTPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resi.. |
|||
Tensile Strength, Ultimate | 22.1 MPa | 3210 psi | |
3M Jet-Weld™ TE-115 HGS Adhesive A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly. Sprayable/extrudable/roll coatable grade with fast set time, ideal for bonding a va.. |