Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.724 GPa | 250.0 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 2518 CU 25% Mineral Filled Polypropylene Multi-Pro 2518 CU is a mineral reinforced polypropylene compound offering overall balanced impact and stiffness properties. This material is specially formulated with UV stabilization for outdoor ex.. |
|||
Flexural Modulus | 1.724 GPa | 250.0 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene Data provided by Multibase. |
|||
Flexural Modulus | 1.724 GPa | 250.0 ksi | ASTM D790 |
Ineos Nova 731G High Impact Polystyrene
(discontinued **) Balance of stiffness and toughness, High impact, USP Class VIApplications: Razor components, Personal care, Consumer goodsIn addition, exposure to gamma radiation in the 2.02-6.06 megarad range ahs .. |
|||
Flexural Modulus | 1.724 GPa | 250.1 ksi | ASTM D790 |
Lucent Polymers CPP-330 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 1.724 GPa | 250.1 ksi | ASTM D790 |
Lucent Polymers TPP-110 Polypropylene, Homopolymer, 10% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 1.724 GPa | 250.0 ksi | ASTM D790 |
Eastman Tenite 285E3720005 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Modulus | 1.724 GPa | 250.0 ksi | ASTM D790 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Modulus | 1.724 GPa | 250.0 ksi | ASTM D790 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |