Polymer Property : Flexural Modulus = 250.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.724 GPa
250.0 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 2518 CU 25% Mineral Filled Polypropylene
Multi-Pro 2518 CU is a mineral reinforced polypropylene compound offering overall balanced impact and stiffness properties. This material is specially formulated with UV stabilization for outdoor ex..
Flexural Modulus 1.724 GPa
250.0 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene
Data provided by Multibase.
Flexural Modulus 1.724 GPa
250.0 ksi
ASTM D790
Ineos Nova 731G High Impact Polystyrene  (discontinued **)
Balance of stiffness and toughness, High impact, USP Class VIApplications: Razor components, Personal care, Consumer goodsIn addition, exposure to gamma radiation in the 2.02-6.06 megarad range ahs ..
Flexural Modulus 1.724 GPa
250.0 ksi
ASTM D790
Eastman Tenite 285E3720005 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 1.724 GPa
250.0 ksi
ASTM D790
Eastman Tenite 307E0V16310 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Modulus 1.724 GPa
250.0 ksi
ASTM D790
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..