Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 8.50 J | 6.27 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene Data provided by Multibase. |
|||
Gardner Impact | 8.50 J | 6.27 ft-lb | J; ASTM D3029-GB, unpainted |
Plaskolite Duraplex® 100% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |