Multibase Multi-Pro® 1510 CNU White Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 1510 CNU White Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.015 - 0.045 cm/cm
0.015 - 0.045 in/in
ASTM D955
Melt Flow 8.5 g/10 min
8.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
73°F; ASTM D256
Gardner Impact 11.298 J
8.3333 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C
201 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C
136 °F
Unannealed; ASTM D648