Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 1510 CNU White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Pro® 4008 RC Medium Impact 40% Glass Filled Polypropylene Multi-Pro 4008 RC is a chemically coupled glass reinforced polypropylene compound exhibiting highest flexural modulus, flex strength and high impact resistance. Heat resistance is high due to highl.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Melt Flow | 8.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific) Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Polimeri Europa Dutral® OCP 2530 PL Ethylene - Propylene Dutral® OCP 2530 PL is an Ethylene - Propylene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.Key F.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific) High impact, extrusion grade polycarbonate/ABS alloy. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer, Uncompounded
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos K44-08-123 HDPE Copolymer with Carbon Black Fortiflex® K44-08-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Melt Flow | 8.5 - 19 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.5 - 19 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D1161 B (SIS) Linear Block Copolymer Description: Kraton D1161 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra.. |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ISO 1133 |
Lucite International Diakon® ST25G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Melt Flow | 8.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific) LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Melt Flow | 8.5 g/10 min @Load 10.0 kg, Temperature 250 °C |
8.5 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Melt Flow | 8.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styron EMERGEâ„¢ 5100 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5100 is a pre-colored, white, ABS resin, having high opacity and excellent toughness intended for manufacture of laser-marketable injection-molded smart cards.Information provided b.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 Conductive GTX, CTE 7 |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific) Conductive GTX, CTE 7 |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Total PPH 3576 BB Polypropylene Homopolymer, Cast Film Polypropylene 3576 BB is recommended for use in non-oriented cast films processes. It contains an optimized level of slip and anti-block additives.3576 BB is intended for food, magazine or textile .. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 TF2 POM Tribological modified grade with addition of 10% PTFE, which causes decreased coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2650 Z2 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 220 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 428 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® 4068FG TPC-ET
(Unverified Data**) Hytrel® 4068FG is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont Performance Polymers |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |