Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638-95 |
Multibase Multi-Pro® 0710 C Brown Polypropylene Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638-95 |
Multibase Multi-Pro® 4013 CU Yellow 40% Filler Content Polypropylene Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638 |
Multibase Nylex™ 1230 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D638 |
Petromont 1100 High Density Polyethylene Resin Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D4745 |
3M Dyneon™ CC698 PTFE 20% Fiberglass/Carbon Filled
(discontinued **) Product Form: Black, pelletized powder. Applications include valve seats.Data provided by Dyneon. |
|||
Tensile Strength, Ultimate | 20.7 - 331 MPa | 3000 - 48000 psi | Average value: 58.7 MPa Grade Count:190 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | 2 in/min.; ASTM D638 |
Ineos H00G-00 Polypropylene Homopolymer A polypropylene homopolymer produced by Ineos utilizing catalyst technology. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. Homopolymer H00G-00 meets certain .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Sylvin Technologies 8600-95 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D882 |
Total PPR 8650 Polypropylene, Random Copolymer ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for orie.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM-D1457 |
CoorsTek PolyGlyde™ 1000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | Molded property |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D412 |
Dow SPECTRIM™ 35-S Reaction Moldable Polymer SPECTRIM™ 35-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Colorite Polymers Self Frosting™ 9011SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Colorite Polymers 9012 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 3072 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 3073 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 3092 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 628 Structural Adhesive Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in SecondsMulti-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 914-A Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 914-A Strain Relief, Wire and Parts Tacking AdhesiveFaster curing, good insulation qualities, shock absorbing, deep .. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 9-20557 Conformal Coating High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-20557 Conformal CoatingFlexible and tough with superior adhesion to a wide range of boards and masks; excellent th.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | |
Dymax 9-911 Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-911 Strain Relief, Wire and Parts Tacking AdhesiveRapid, high strength, designed for difficult substrates, resists.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | Bond strength to glass |
Dymax Light Weld® 402 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Tensile Strength, Ultimate | 20.7 - 34.5 MPa | 3000 - 5000 psi | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Tensile Strength, Ultimate | 20.7 - 24.1 MPa | 3000 - 3500 psi | TM R050-36 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Tensile Strength, Ultimate | 20.7 - 24.1 MPa | 3000 - 3500 psi | TM R050-36 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Tensile Strength, Ultimate | 20.7 MPa | 3000 psi | ASTM D412 |
MF-5001 Polyurethane-based Biomedical Elastomer |