Polymer Property : Linear Mold Shrinkage = 0.045 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.015 - 0.045 cm/cm
0.015 - 0.045 in/in
ASTM D955
Multibase Multi-Pro® 1510 CNU White Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Linear Mold Shrinkage 0.015 - 0.045 cm/cm
0.015 - 0.045 in/in
0.125 in; ASTM D955
Entec Hypel® PELD8/.920 LDPE
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..