Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 1508 M Polypropylene Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Pro® 4008 RC Medium Impact 40% Glass Filled Polypropylene Multi-Pro 4008 RC is a chemically coupled glass reinforced polypropylene compound exhibiting highest flexural modulus, flex strength and high impact resistance. Heat resistance is high due to highl.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 50-0863 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific) High impact, extrusion grade polycarbonate/ABS alloy. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 8.5 - 11 g/10 min | 8.5 - 11 g/10 min | ASTM D1238 |
Kolon KOCETAL® MS301 Wear Modified Acetal Resin Molybdenum disulfide added, improved wear property. Applications: Products for low noise and friction against metal. Information provided by API-Kolon. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos J60-800-178 HDPE A high density polyethylene homopolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still and sparkling water.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos K44-08-123 HDPE Copolymer with Carbon Black Fortiflex® K44-08-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Melt Flow | 8.5 - 19 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.5 - 19 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D1161 B (SIS) Linear Block Copolymer Description: Kraton D1161 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra.. |
|||
Melt Flow | 8.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific) LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 8.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ISO 1133 |
Wico Plast Wicolon 805 Polycarbonate ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ISO 1133 |
Wico Plast Wicolon 807 Polycarbonate, U.V. Stabilized ApplicationsInjection moldingCharacteristics:U.V. stabilizedAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSC 536 Polystyrene Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
GB/T 3682 |
Chengdu Polyster KP-200-40 Silicone Masterbatch KP-200 series silicone masterbatches are white pellets or white powder which made from ultra-high molecular weight polysiloxane, used by plastics as processing aids and impart expected silicone bene.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Melt Flow | 8.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Dow AIM® 4810 High Impact Styrenic Resin AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ LD 706.15 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for specialty molding, extrusion and compounding applications.Availability: Latin America, Nor.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer Hot melt adhesive |
|||
Melt Flow | 8.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polyrex® PG-33 Polystyrene Standard grade |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 K POM Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 3090(K) POM Copolymer, 27% glass fiber reinforced POM-GF27Information provided by BARLOG plastics GmbH. |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ASTM D1238 |
Asahi Kasei Thermylene® P6-15FG-1734 15% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |