Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 1510 CNU White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2520 XU Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Multibase Nylex™ 2185 FR V0 Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hifaxâ„¢ CB259 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB259 medium high melt flow, 1,600 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact r.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
LyondellBasell Hostacomâ„¢ 63A6-4 Polypropylene Homopolymer Description: Hostacomâ„¢ 63A6-4 medium high melt flow, 2,200 MPa flexural modulus, 40% calcium carbonate-filled polypropylene homopolymer has an excellent combination of properties, chemical resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantTPCI# 1039121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackTPCI# 9224121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR UV BK Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceUL File Number: E157318Appearance: BlackTPCI# 9224121Information provided by TP Compos.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR V2 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ASTM D648 |
Spartech Millennium IV Glass Filled ABS Structural Sheet Description: Structural SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8004 FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8004 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8004 UV MB Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceTPCI# 6816121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8010 Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8012 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8014 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8002 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8004 Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS FR IM Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS HH BK MB Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS IM Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | 0.250 inch; Unannealed; ASTM D648 |
TPI Porene® GA300 High Flow Grade, High Gloss ABS INJECTION MOLDING. APPLIANCES, BUSINESS EQUIPMENT, ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Inform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ISO 75-2/B |
ExxonMobil Exxtral™ BMU 143 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ISO 75-2/B |
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ASTM D648 |
Aclo Accutech ABS ABS831G10L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0436W10L Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ASTM D648 |
Americas Styrenics STYRON A-TECH® 1290 High Impact Polystyrene Product CharacteristicsEasy processingGood impact resistanceESCRFood Contact CompliantUL Classification 94HBTypical ApplicationsCreamer and yot containersExtrusion/ thermoformingInformation provided.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C @Thickness 3.17 mm |
201 °F @Thickness 0.125 in |
Unannealed; ISO 75-2-92 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |