Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 8102 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 8102 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.065 g/cc
0.03848 lb/in³
ASTM D792
Melt Flow 1.5 g/10 min
1.5 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 sec; ASTM D-2240
Tensile Strength, Ultimate 9.00 MPa
1310 psi
ASTM D412
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Flexural Modulus 0.490 GPa
71.1 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 35.0 kN/m
200 pli
ASTM D624