Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.065 g/cc | 0.03848 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8102 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.065 g/cc | 0.03848 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Density | 1.065 g/cc | 0.03848 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Density | 1.065 g/cc | 0.03848 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Density | 1.065 g/cc | 0.03848 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP V1000UXC PA LNP* Thermotuf* V1000UXC is a compound based on Nylon resin. Added features of this material include: UV Stabilized. |