Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 10 - 15 g/10 min
10 - 15 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
10 sec; ASTM D-2240
Tensile Strength, Ultimate 8.30 MPa
1200 psi
ASTM D412
Elongation at Break >= 600 %
>= 600 %
ASTM D412
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Tear Strength >= 8.30 kN/m
>= 47.4 pli
ASTM D624
Copyright © lookpolymers.com All Rights Reserved