Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 8.30 kN/m | >= 47.4 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7318 GREY The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 8.31 kN/m | 47.4 pli | BS EN ISO 8067 1995 |
Zotefoams Plastazote® HD115 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |