Multibase Multi-ABS 802 Natural Extrusion Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer Multibase
Trade Name Multi-ABS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-ABS 802 Natural Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955-89
Melt Flow 2.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
ASTM D785-95
Tensile Strength, Ultimate 39.3 MPa
5700 psi
ASTM D638-95
Elongation at Break 40 %
40 %
ASTM D638-95
Flexural Strength 50.0 MPa
7250 psi
ASTM D790-95
Flexural Modulus 1.862 GPa
270.1 ksi
RT; ASTM D-790-95
Izod Impact, Notched 4.00 J/cm
7.49 ft-lb/in
ASTM D256-93a
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
injection molded unannealed; ASTM D-648-95
102 °C
216 °F
injection molded annealed; ASTM D-648-95
Vicat Softening Point 91.0 °C
196 °F
ASTM D1525-95
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in