10 percent active, water dilutable silicone emulsion designed to control foam in water based industrial processes.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc

@Temperature 25.0 °C
1.00 g/cc

@Temperature 77.0 °F
pH 4.0
4.0
Viscosity 150 cP
150 cP
dynamic
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Active Content (%) 10
Color white
Compatibility Aqueous Systems
Non-Ionic yes
Water Dispersible yes
Users viewing this material also viewed the following: