A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® ABPP-05 Antiblock is an antiblock concentrate containing 5% synthetic silica based in homopolymer polypropylene. This masterbatch is designed to provide high clarity, low haze, optimum dispersion, and consistent COF development when used in the skin layers of cast, blown and BOPP film applications. POLYBATCH® ABPP-05 is generally recommended for use at 2 to 3% addition levels depending upon customer specific requirements. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ash 5.0 %
5.0 %
ASTM D2765
Descriptive Properties Value Comments
Moisture 1000
ppm, ASTM D789 @ 190°C
Pellet Count 45
pellets/gram