Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.862 GPa | 270.1 ksi | Secant 20% max load; ASTM D-790-95 |
Multibase Multi-Pro® 3019 CXUW High Gloss 30% TiO2 Filler Content Polypropylene Multi-Pro 3019 CXUW is a mineral reinforced polypropylene compound exhibiting high stiffness and impact characteristics. This material was specially formulated with UV stabilization for outdoor app.. |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | RT; ASTM D-790-95 |
Multibase Multi-ABS 802 Natural Extrusion Grade Data provided by Multibase. |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | ASTM D790 |
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and.. |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | ASTM D790 |
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | ASTM D790 |
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | ASTM D790 |
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, .. |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | tangent; ASTM D790 |
Entec Hypro™ PPH-CC20 Natural Homopolymer Polypropylene, 20% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | tangent; ASTM D790 |
Entec Hypro™ PPH-T10 Homopolymer Polypropylene, 10% Talc Reinforced Information provided by Entec |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | ASTM D790 |
Diamond Polymers NYLON 6650HSL Black Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | ASTM D790 |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Modulus | 1.862 GPa | 270.1 ksi | ASTM D790 |
Lucent Polymers TPP-220 Polypropylene, 20% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |