Material Notes:
Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® is a pre-product sorted according to type and color, which is produced through a patented separating process.Information provided by MTM Plastics GmbH.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ISO 1183
Moisture Absorption <= 0.100 %
<= 0.100 %
Melt Flow >= 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
>= 20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash <= 2.0 %
<= 2.0 %
Ignition Residue after 650°C; ISO 1172
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
DIN 53505
Tensile Strength, Yield >= 24.0 MPa
>= 3480 psi
50 mm/min; ISO 527
Elongation at Yield >= 18 %
>= 18 %
50 mm/min; ISO 527
Tensile Modulus >= 1.10 GPa
>= 160 ksi
1 mm/min; ISO 527
Charpy Impact, Notched >= 0.300 J/cm²

@Temperature -23.0 °C
>= 1.43 ft-lb/in²

@Temperature -9.40 °F
edgewise; ISO 179
>= 0.650 J/cm²

@Temperature 23.0 °C
>= 3.09 ft-lb/in²

@Temperature 73.4 °F
edgewise; ISO 179