PolyOne Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedIgnition ResistantNon-HalogenatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 64.8 MPa
9400 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 0.60 %
0.60 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 13.02 GPa
1888 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 0.278 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.520 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
All Colors; 0.125 in.
Processing Properties Metric English Comments
Melt Temperature 232 - 260 °C
450 - 500 °F
Molding
Mold Temperature 82.2 - 93.3 °C
180 - 200 °F
Drying Temperature 93.3 °C
200 °F
Dry Time 4 hour
4 hour
Descriptive Properties Value Comments
Product Form Pellets