Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® LB560401 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® LB560401 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPetrothene LB560401 exhibits good stiffness and environmental stress crack resistance. Typical applications include household chemical and personal care product bottles.Regulatory StatusLB560401 meets the requirements of the Food and Drug Administration, regulation 21 CFR 1 77.1 520.Processing TechniquesSpecific recommendations for processing LB560401 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
ASTM D2561
ESCR 100% Igepal® 25 hour
25 hour
ASTM D1693
Melt Flow 0.35 g/10 min
0.35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Tensile Impact 61.4 J/cm
115 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C
165 °F
ASTM D648
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Compliance Properties Metric English Comments
FDA Yes
Yes
Users viewing this material also viewed the following: