Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin Molded Plaque Properties.Applications: drums, large industrial parts.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693 |
NOVA Chemicals Novapol® HB-W555-AC PE Blow Molding Resin High molecular weight, High rigidity, Excellent impact strength, Excellent ESCR, Used in high purity chemical packagingInformation provided by NOVA Chemicals. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F<sub>0</sub>; ASTM D1693/B |
Reliance Industries Relene S42005 Polyethylene Wire and cable High Density Polyethylene grade. Characteristics: excellent processing, superior physical/electrical properties, good environmental stress crack resistance. Applications: recommended .. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F-50; 10% Igepal Cond. B; ASTM D1693 |
ExxonMobil Escorene® LL-8361 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-8 type protection, Good flowUses: Consumer items, Potable water tanks, Laundry tubs |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | (10% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L64220UT1 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Large tanks, material handling equipment and industrial rotational molding applications.Formolene L64220U is fully heat and UV stabilized.Meets all requirements of the .. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-701 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10.5% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughnes.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-706 High EVA Cast Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.3% vinyl acetate copolymer film resin designed for coextruded cast film applications.Applications: Coextruded meat packaging film; Sealant in c.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-722 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-723 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-781 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymer for specialty compounding applications. The resin provides excellent stress cracking and flexibility, and allows outs.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition B; ASTM D1693 |
ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8400 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8461 is fully formu.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 102-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 153-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 15313-003 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F<sub>50</sub>; ASTM D2561 |
LyondellBasell Petrothene® LR732031 High Density Polyethylene ApplicationsPETROTHENE LR 7320-31 is a high density polyethylene resin that exhibits an excellent balance of stiffness and environmental stress crack resistance. This resin has outstanding extrusio.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50; ASTM D1693 |
LG Chemical LUTENE FB0300 LDPE Blown Film Grade Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50; ASTM D1693 |
LG Chemical SEETEC PB150 HDPE Features: This high molecular weight, hexane copolymer is tailored for high impact blow-molded containers that require:Excellent processabilityHigh impact strength at low temperatureOutstanding stre.. |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | |
JPJ Technologies 7800M HDPE Extrusion Information provided by JPJ Technologies |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | GOST 13518 |
Sibur 15303-003 Low Density Polyethylene For production of films and film articles, including thermoset films, thin films, food contact grade films
(including tight packing), general-purpose films, and bags. |
|||
Environmental Stress Crack Resistance | >= 500 hour @Temperature 50.0 °C |
>= 500 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1693 |
SCG Chemicals EL-Proâ„¢ P401S Polypropylene Flat Yarn/Sheet Key Characteristics: Excellent mechanical propertiesRecommended Applications:Stretch tape for jumbo woven sheetMonofilament for rope and sheetInformation provided by SCG Chemicals |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | Antarox 10%, F50; ASTM D1693-A |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50; ASTM D2561 |
CPC - Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE) Grip-X is a UV stabilized high density polyethylene (HDPE) sheet formulated to meet demanding conditions of the marine industry. Grip-X is manufactured with a special surface treatment and stipulate.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50; ASTM D2561 |
CPC - Vycom SEABOARD™ Premier High density polyethylene (HDPE) Seaboard High Density Polyethylene (HDPE) is the toughest marine grade polymer sheet available. This UV stable product has scratch resistance, excellent impact, and stiffness, yet it is easy to mach.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F<sub>o</sub>; Compression molded parts prepared according to ASTM D 1928, condition A.; ASTM D1693 |
Dow FINGERPRINT™ DFDA-7510 NT Linear Low Density Polyethylene Resin FINGERPRINT™ DFDA-7510 NT resin is produced using UNIPOL™ process technology. It is intended for use in micro irrigation tube, durable hose and tube, profile extrusion, and injection molded fitti.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F<sub>o</sub>; Compression molded parts prepared according to ASTM D 1928, condition A.; ASTM D1693 |
Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-7441 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in hose and tube applications. It also has utility in gasketing, spiral wound hose, and corrugated hose .. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | ASTM D1693 cond. B 10% lgepal |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-730 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-724 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty compounding applications. Outstanding heat sealability along with excellent strength properties .. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 153-11K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |