Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CM003 Polypropylene Impact Copolymer CM003 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes.Applications: Extrusion ProcessesInformation provided .. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | Condition not noted.; ASTM D1238 |
DuPont Elvax® 3129 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 10 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | ExxonMobil Method |
ExxonMobil Escorene® LD 712.06 Film Resin
(discontinued **) Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg |
0.35 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Global G-2855 High Density Polyethylene, Blow Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CM003P Polypropylene Impact Copolymer COPYLENE® CM003P is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes.Applications: Extrusion ProcessesInformati.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | ASTM D1238 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LB5604 High Density Polyethylene ApplicationsThe PETROTHENE LB 5604 series of polyethylene resins exhibits good stiffness and environmental stress cracking resistance. Typical applications include household chemical and person car.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LB560401 High Density Polyethylene ApplicationsPetrothene LB560401 exhibits good stiffness and environmental stress crack resistance. Typical applications include household chemical and personal care product bottles.Regulatory Status.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LM600500 High Density Polyethylene ApplicationsPETROTHENE LM 6005-00 resin is especially designed for water, milk, and juice bottles. It exhibits excellent rigidity and good processability.Regulatory StatusLM 6005-00 meets the requi.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | ASTM D1238 |
I. Stern IS-35955 High Density Polyethylene, Blow Molding Grade Features:IS-35955 is designed for applications requiring excellent stiffness and stress crack resistance properties.Meets all requirements of the U. S. Food and Drug Administration as specified in 2.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos B50-35H-011 HDPE Ineos B50-35H-011 is a high density polyethylene copolymer developed for blow molding applications. It is recommended for use in applications which require a combination of high top load strength a.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 5-8250 W 50% Chalk-Filled High Density Polyethylene INNOPOL® CS 5-8250 W is a 50% chalk-filled compound based on high density polyethylene.INNOPOL® CS 5-8250 W is developed for packaging film production.All information provided by INNO-COMP. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | |
JPJ Technologies 5200B HDPE Blow Molding Information provided by JPJ Technologies |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | ASTM D1238 |
UBE R300 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | Condition not noted.; ASTM D1238 |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 3135XZ Ethylene Vinyl Acetate DuPont™ Elvax® 3135XZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applicati.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 670 Ethylene Vinyl Acetate DuPont™ Elvax® 670 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 670 resins can be used for the following applications: molding, compounding .. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Total 5502 HDPE, blow molding, pipe Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HB5202A Blow Molding HDPE High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5202A is designed for applications requiring excellent stiffness and stress crack resistance propertiesAppl.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HB5502F Blow Molding HDPE High Density Polyethylene Hexene Copolymer with Synthetic Antistat Formolene® HB5502F HDPE resin is designed for applications requiring excellent stiffness and stress crack resistance properties. I.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M 2704 EP S01 is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2704 EP S01 can be.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | ASTM D1238 |
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Fainplast Compounds Ethylplus 619 LD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack LDPE SheathingInformation provided by Fainplast.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of product.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HB5502B2 Blow Molding HDPE Hexene CopolymerApplications: Pharmaceutical Packaging; Personal Care Products;
Bleach and Detergents Industrial; and Chemicals & PartsFormolene® HB5502B2 is designed for applications requiring ex.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
(discontinued **) AG45-004 is a blow molding high density polyethylene which offers exceptional stress crack resistance and impact performance. It contains an antistat which permits this resin to be used in all food.. |
|||
Melt Flow | 0.35 g/10 min | 0.35 g/10 min | Exxon Method (I2). HLMI (I21) is 20 g/10 min. |
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom.. |