Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 61.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648
Network Polymers NPP 25-0616
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648
ExxonMobil LL 8450 Rotational Molding Resin  (discontinued **)
LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
LyondellBasell Lupolen® 3821 D MDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight
For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight
For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648
LyondellBasell Alathon® M4612 High Density Polyethylene
ApplicationsALATHON M 4612 is a copolymer that provides outstanding ESCR and low temperature impact strength. Typical applications include food containers, seat hinges, tube headers.Regulatory Stat..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648
LyondellBasell Alathon® M5040 High Density Polyethylene
ApplicationsALATHON M 5040 is a copolymer with broad molecular weight distribution. This resin exhibits excellent color, low odor, and good processing stability. Typical applications for this res..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648-97
Ipiranga Petrochem MB 0434 LS-L MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648-97
Ipiranga Petrochem MB 0435 MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU
LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648
SK Chemicals SKYPEL P137DW Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C

@Thickness 3.20 mm
142 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy
DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C

@Thickness 3.20 mm
142 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy
DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C

@Thickness 3.20 mm
142 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy
DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C

@Thickness 3.20 mm
142 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy
DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C

@Thickness 3.20 mm
142 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy
DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C

@Thickness 3.20 mm
142 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy
DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
Covestro Desmopan® 460 Thermoplastic Polyurethane
Desmopan 460 is a TPU on the basis of a special ester.Applications: Bearing shells, gear wheels, seals, cable connectors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience w..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648
ExxonMobil LL 8450.31 Rotational Molding Resin
Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
ASTM D648
ExxonMobil LLP8450.31 Rotational Molding Resin
LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir..
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C
142 °F
90 Minute UV Cure; ASTM D648
3D Systems Accura® SI 40 Plastic for the SLA® 250 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..
Copyright © lookpolymers.com All Rights Reserved