LyondellBasell Hifaxâ„¢ AB220GC/1 Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Hifax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ AB220GC/1 Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: fractional melt flow, high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, high flexural modulus, high impact strength, good weatherability, good processabilityApplications: extruded profiles and luggage rack insertsDescription: Hifax AB220GC/1 fraction melt flow, UV-stabilized mineral-filled, extrusion grade thermoplastic olefin resin has an excellent balance of stiffness, impact strength, weather resistance and processability. It was designed primarliy for extruded automotive exterior profile applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792B
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Tool, Montell
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2440
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
Tangent at 0.05 in/min; ASTM D790A
Gardner Impact 24.0 J

@Temperature -30.0 °C
17.7 ft-lb

@Temperature -22.0 °F
ASTM D3029
Impact Test 24.0 J

@Temperature -30.0 °C
17.7 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
Tear Strength 160 kN/m
913 pli
ASTM D624