Polymer Property : Tear Strength = 160 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 160 kN/m
913 pli
Die C; ASTM D624
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane
This high-performance quasi-polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhib..
Tear Strength 160 kN/m
915 pli
DIN 53.515
Lubrizol Advanced Materials Pearlthane® ECO D20N55D Thermoplastic Polyurethane  (discontinued **)
PEARLTHANE® ECO D20N55D is a 55 Shore D, High Performance natural TPU based on Renewable Sources with ca. 35% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicati..
Tear Strength 160 kN/m
913 pli
ASTM D624
LyondellBasell Hifaxâ„¢ AB220GC/1 Thermoplastic Olefin Resin
Key Features: fractional melt flow, high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, high flexural modulus, high impact strength, good weatherability, good processabilityAppl..
Tear Strength 160 kN/m
910 pli
ASTM D624
LyondellBasell Hifaxâ„¢ RTA3263EUV/1 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ RTA3263EUV/1 fractional melt flow, 1,700 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent b..
Tear Strength 160 kN/m
913 pli
ASTM D1004
SK Chemicals SKYPEL M555DH General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tear Strength 160 kN/m
913 pli
ASTM D624
Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.
Tear Strength 160 kN/m
913 pli
with incision; ISO 34B
Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 160 kN/m
913 pli
ASTM D624
C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Tear Strength 160 kN/m
913 pli
DIN ISO 34-1/Bb
BASF Elastollan C 59 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Tear Strength >= 160 kN/m
>= 913 pli
ISO 34
Austin Novel Materials Texalan® 264D Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tear Strength >= 160 kN/m
>= 913 pli
ISO 34
Austin Novel Materials Texalan® 564D Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tear Strength >= 160 kN/m
>= 913 pli
ISO 34
Austin Novel Materials Texalan® 364D Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tear Strength 160 kN/m
913 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-1564 Polyester Based TPU
Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 160 kN/m
913 pli
ASTM D624
BASF Elastollan® M95A55 Polyester Type Polyurethane Elastomer
The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl..
Tear Strength 160 kN/m
913 pli
DIN 53515
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..