Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 160 kN/m | 913 pli | Die C; ASTM D624 |
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane This high-performance quasi-polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhib.. |
|||
Tear Strength | 160 kN/m | 913 pli | ASTM D624 |
LyondellBasell Hifaxâ„¢ AB220GC/1 Thermoplastic Olefin Resin Key Features: fractional melt flow, high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, high flexural modulus, high impact strength, good weatherability, good processabilityAppl.. |
|||
Tear Strength | 160 kN/m | 913 pli | ASTM D1004 |
SK Chemicals SKYPEL M555DH General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tear Strength | 160 kN/m | 913 pli | ASTM D624 |
Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Tear Strength | 160 kN/m | 913 pli | with incision; ISO 34B |
Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 160 kN/m | 913 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 160 kN/m | 913 pli | DIN ISO 34-1/Bb |
BASF Elastollan C 59 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tear Strength | >= 160 kN/m | >= 913 pli | ISO 34 |
Austin Novel Materials Texalan® 264D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tear Strength | >= 160 kN/m | >= 913 pli | ISO 34 |
Austin Novel Materials Texalan® 564D Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tear Strength | >= 160 kN/m | >= 913 pli | ISO 34 |
Austin Novel Materials Texalan® 364D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tear Strength | 160 kN/m | 913 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1564 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 160 kN/m | 913 pli | ASTM D624 |
BASF Elastollan® M95A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Tear Strength | 160 kN/m | 913 pli | DIN 53515 |
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |