Material Notes:
Description: DEXFLEX® 810-1 is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. DEXFLEX® 810-1 was designed to exceed the requirements of US 5-mph bumper-impact regulations. Applications: Bumper fascias, and other large components that must exhibit durable paintability in exterior body colors Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ISO 1183
Linear Mold Shrinkage 0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
as molded; ISO 294
0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
after bake; ISO 294
Melt Flow 9.0 g/10 min
9.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 0.790 GPa
115 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
50.0 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228