Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.930 g/cc @Temperature 22.8 °C |
0.930 g/cc @Temperature 73.0 °F |
ASTM D792 |
Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
LG Chemical KEYFLEX TO1192A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical |
|||
Specific Gravity | 0.930 - 0.940 g/cc | 0.930 - 0.940 g/cc | |
Inhance Fluoro-Seal INHANCE® UH-1500 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ISO 2781 |
Kraton® Cariflex™ IR0401 SU Polyisoprene Rubber Latex Description: Cariflex IR0401 SU Latex is a water-based emulsion of an anionically polymerized polyisoprene with a high cis-1,4 content, high molecular weight and a high linearity. The emulsion also.. |
|||
Specific Gravity | 0.930 g/cc @Temperature 25.0 °C |
0.930 g/cc @Temperature 77.0 °F |
|
Multibase Dow Corning® MB25-504 Siloxane Additive DOW CORNING MB25-504 Masterbatch is a pelletized formulation containing 25% of a high molecular weight siloxane polymer dispersed in HIPS polymer. It is designed to be used as an additive in HIPS co.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1949A-55NT Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Teknor Apex Uniprene® 50D Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7100-40D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Teknor Apex Uniprene® UN-2420D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Specific Gravity | 0.930 - 0.960 g/cc | 0.930 - 0.960 g/cc | |
Westlake Epolene® E-14P Oxidized Low Molecular Weight Polyethylene Polymer Description: The Epolene E-14P is a low molecular-weight, low-density, oxidized polyethylene powder. It is useful as a lubricant in processing rigid and flexible polyvinyl chloride (PVC) and as a pr.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ AO-25 Antioxidant Masterbatch Based in LDPE DescriptionPOLYBATCH® AO-25 is a general purpose antioxidant masterbatch based in LDPE. ApplicationThis concentrate is designed for use in polyethylene film and molding applications for improving .. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ MAS-25 Concentrate Based In LDPE DescriptionPOLYBATCH® MAS-25 is an organic antislip concentrate based in LDPE. This masterbatch is designed for use in moderate to heavy gauge film and sheet applications where extreme antislip p.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate DescriptionPOLYBATCH® ABPP-05 Antiblock is an antiblock concentrate containing 5% synthetic silica based in homopolymer polypropylene. This masterbatch is designed to provide high clarity, low haz.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | DIN 53479 |
Dynasol Solprene® 1217 Solution Styrene-Butadiene Rubber (SSBR) Solprene1217 is a linear random-block styrene/butadiene copolymer having 25% of styrene content, 17.5% present as a polystyrene block. It has a non-staining antioxidant system, BHT/TNPP free, FDA ap.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792/ISO 1183 |
Braskem UTEC® 4040 Ultra High Molecular Weight Polyethylene Applications which require a good combination between impact and wear resistance - technical and porous parts, filters, compression molded sheets.Information provided by Braskem. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | |
AlphaGary AlphaSeal™ 07-193-C Natural Thermoplastic Elastomer AlphaSeal™ 07-193-C Natural is recommended for the skin over extruded foamed corks. AlphaSeal is formulated for low taste and low odor and exhibits good elastic recovery, abrasion resistance and l.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ISO 2782 |
AlphaGary Evoprene™ 019 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8211-55M300 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
E-Polymers EFLEX® I2010 Ionomer I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnes.. |
|||
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ISO 2781 |
Kraton® D1119 B (SIS) Linear Triblock Copolymer Description: Kraton D1119 B is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from South America in the physical form identified: .. |