Mechanical Properties Metric English Comments
Tensile Impact 152 J/cm
285 ft-lb/in
ASTM D1822
LyondellBasell Alathon® L5332CP High Density Polyethylene
ApplicationsALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resis..