Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9410 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good TrimabilityApplications:Phar.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 35BP HDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Melt Flow | 0.32 g/10 min | 0.32 g/10 min | ASTM D1238 |
LyondellBasell Alathon® L5332CP High Density Polyethylene ApplicationsALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resis.. |
|||
Melt Flow | 0.32 g/10 min | 0.32 g/10 min | ASTM D1238 |
LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applic.. |
|||
Melt Flow | 0.32 - 0.58 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.32 - 0.58 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 7040 G HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem BF 0323 HC LDPE Blown Film Extrusion Polyethylene Description: BF0323HC is a high molecular weight grade produced under high pressure. Films obtained with this product show excellent mechanical and optical properties38µm film gauge, obtained in 75.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem BF 0323/12 HC LDPE Blown Film Extrusion Polyethylene Description: BF0323/12 is a high molecular weight LDPE produced under high pressure technology. Films obtained with this product show outstanding optical properties, excellent mechanical properties,.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9512/HiD® 9513 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Syncure™ S1075A Polyethylene, Crosslinked (XLPE) Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1074A / 5 phr S1.. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BF0323/12HC Blown Film Extrusion Low Density Polyethylene Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem. |
|||
Melt Flow | 0.32 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BF0323HC Blown Film Extrusion Low Density Polyethylene Heavy-duty bags; Agriculture, Coextruded and shrink films for pallets.Information provided by Braskem. |