Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 9.45 g/cc
9.45 g/cc
Density 9.45 g/cc
0.342 lb/in³
Thermal Properties Metric English Comments
Melting Point 627 - 635.0 °C
1160 - 1175 °F
Solidus 627 °C
1160 °F
Liquidus 635.0 °C
1175 °F
Maximum Service Temperature, Air 204 °C
400 °F
continuous
316 °C
600 °F
intermittent
Component Elements Properties Metric English Comments
Cadmium, Cd 17 - 19 %
17 - 19 %
Copper, Cu 14.5 - 16.5 %
14.5 - 16.5 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 49 - 51 %
49 - 51 %
Zinc, Zn 14.5 - 18.5 %
14.5 - 18.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000700 ohm-cm
0.00000700 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 649 - 760 °C
1200 - 1400 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Yellow
Electrical Conductivity (% IACS) 23.9