Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.45 g/cc | 0.341 lb/in³ | |
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin.. |
|||
Density | 9.45 g/cc | 0.342 lb/in³ | |
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s.. |