Polymer Property : Processing Temperature = 1400 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 618.3 - 760 °C
1145 - 1400 °F
Brazing Temperature
Lucas-Milhaupt Silvally® 45 Flux Coated Rod Brazing Alloy
Silvaloy 45 FC is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joinin..
Processing Temperature 618.3 - 760 °C
1145 - 1400 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy
Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining s..
Processing Temperature 651.7 - 760 °C
1205 - 1400 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® A56T Brazing Alloy
Silvaloy A56T has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on some applications. ..
Processing Temperature 651.7 - 760 °C
1205 - 1400 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® A56T Flux Coated Rod Brazing Alloy
Silvaloy A56T Flux Coated Rod has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on som..
Processing Temperature 688 - 760 °C
1270 - 1400 °F
Brazing Range
Lucas-Milhaupt EASY FLO 3 Carbide Brazing Alloy
Easy-Flo 3 is recommended for use on stainless steels subject to chloride corrosion, such as marine hardware, fishing tackle, and some dairy equipment cleaned with bleaching solutions and other equi..
Processing Temperature 651.7 - 760 °C
1205 - 1400 °F
Brazing Temperature
Lucas-Milhaupt Silvacore® A56T Flux Cored Brazing Alloy
Silvaloy A56T Flux Cored has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on some app..
Processing Temperature 649 - 760 °C
1200 - 1400 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy
Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s..