Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxon Hyjet IV-A

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxon Hyjet IV-A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exxon HyJet IV-Aplus is a fire-resistant phosphate ester hydraulic fluid designed for use in commercial aircraft. It is the best-performing Type IV fluid and offers to a great extent many of the performance capabilities of Type V fluids, including high temperature stability, low density, and rust protection. It is superior to all other Type IV fluids in these respects. Exxon HyJet IV-Aplus meets the specifications of all major aircraft manufacturers and SAE AS1241.Exxon HyJet IV-Aplus fire-resistant aviation hydraulic fluid is used in commercial aircraft hydraulic systems where phosphate hydraulic fluids are recommended. Exxon HyJet IV-Aplus meets or exceeds the following industry and builder specifications.  It is approved against the aircraft manufacturer requirements and is included in their Qualified Products Lists.
Physical Properties Metric English Comments
Specific Gravity 0.996 g/cc
0.996 g/cc
25°C; ASTM D4052
Density 1.001 g/cc

@Temperature 15.6 °C
0.03616 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 320
320
Index; ASTM D2270
Viscosity Measure 1320 cSt

@Temperature -54.0 °C
1320 cSt

@Temperature -65.2 °F
Kinematic Viscosity; ASTM D445
Kinematic Viscosity at 40°C (104°F) 10.55 cSt
10.55 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 3.57 cSt
3.57 cSt
ASTM D445
Evaporation Loss 15 %
15 %
6 hr @ 71°C
Mechanical Properties Metric English Comments
Bulk Modulus 1.448 GPa
210.0 ksi
Isothermal secant at 100°F/3000psi
Thermal Properties Metric English Comments
CTE, linear 860 µm/m-°C

@Temperature 25.0 - 100 °C
478 µin/in-°F

@Temperature 77.0 - 212 °F
Specific Heat Capacity 1.72 J/g-°C
0.410 BTU/lb-°F
Thermal Conductivity 0.138 W/m-K

@Temperature 40.0 °C
0.957 BTU-in/hr-ft²-°F

@Temperature 104 °F
Pour Point <= -62.0 °C
<= -79.6 °F
ASTM D97
Flammability Test 185
185
Fire Point [°C]
>= 427
>= 427
Auto Ignition [°C]
Flash Point 174 °C
345 °F
ASTM D92
Component Elements Properties Metric English Comments
Calcium, Ca 0.011 %
0.011 %
Chlorine, Cl <= 0.00070 %
<= 0.00070 %
H2O 0.10 %
0.10 %
Potassium, K 0.0037 %
0.0037 %
Sodium, Na 0.00 %
0.00 %
Sulfur, S 0.022 %
0.022 %
Electrical Properties Metric English Comments
Electrical Resistivity 71.4 ohm-cm

@Temperature 20.0 °C
71.4 ohm-cm

@Temperature 68.0 °F
Chemical Properties Metric English Comments
Total Acid Number 0.040
0.040
mgKOH/g; ASTM D974
Descriptive Properties Value Comments
Foam Sequence I, ASTM D1137 0/0
Foam Sequence II, ASTM D893 0/0
Foam Sequence III, ASTM D893 0/0
Particle Count, NAS 1638 Class 4
Sonic Shear Stability, KV change % 22
@ 40°C
Users viewing this material also viewed the following: