Polymer Property : Specific Gravity = 9.45 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 9.45 g/cc
9.45 g/cc
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy
Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s..