Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 9.45 g/cc | 9.45 g/cc | |
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s.. |