Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.48 - 9.68 g/cc | 0.342 - 0.350 lb/in³ | |
MarkeTech Cu/Mo/Cu 1:2:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Density | 9.46 g/cc | 0.342 lb/in³ | |
MarkeTech Cu/Mo70-Cu30/Cu 1:4:1 Laminated Sheet Cu/Mo/Cu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated he.. |
|||
Density | 9.47 g/cc | 0.342 lb/in³ | |
Indium Corp. Indalloy 140 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.48 g/cc | 0.342 lb/in³ | |
Indium Corp. Indalloy 179 Silver Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.48 g/cc | 0.342 lb/in³ | |
Indium Corp. Indalloy 47 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.48 g/cc | 0.342 lb/in³ | |
Indium Corp. Indalloy 68 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.47 g/cc | 0.342 lb/in³ | |
Indium Corp. Indalloy 101 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.45 g/cc | 0.342 lb/in³ | |
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s.. |