Polymer Property : Electrical Resistivity = 0.00000700 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000700 ohm-cm
0.00000700 ohm-cm
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin..
Electrical Resistivity 0.00000700 ohm-cm
0.00000700 ohm-cm
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy
Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s..