Material Notes:
Type: Estane® S395A is a Shore 95A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength, Ultimate 46.1 MPa
6680 psi
ASTM D412
Tensile Strength, Yield 13.7 MPa
1990 psi
at 100% elongation; ASTM D412
27.5 MPa
3980 psi
at 300% elongation; ASTM D412
Elongation at Break 530 %
530 %
ASTM D412
Tear Strength 157 kN/m
896 pli
Die C; ASTM D624
Abrasion 30
30
mm<sup>3</sup> loss; ISO 4649
Compression Set 15 %

@Temperature 23.0 °C,
Time 79200 sec
15 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
45 %

@Temperature 70.0 °C,
Time 79200 sec
45 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Processing Properties Metric English Comments
Feed Temperature 180 - 195 °C
356 - 383 °F
Nozzle Temperature 190 - 205 °C
374 - 401 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Pressure 8.27 - 13.8 MPa
1200 - 2000 psi
Hold Pressure 5.52 - 9.65 MPa
800 - 1400 psi
Back Pressure 0.207 - 0.552 MPa
30.0 - 80.0 psi
Cycle Time - Injection 20 - 30 sec
20 - 30 sec
Screw Speed 160 - 200 rpm
160 - 200 rpm
Descriptive Properties Value Comments
Injection time (s) 10-15
Metering Zone 185-200°C