Processing Properties Metric English Comments
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUCON PS4200 ABS+CF
Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch..
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUCON SP9306FL sPS+MF
Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 ..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant
Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)
Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG ..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose
Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMID GP3400B(W) PA66+MF40%, General Purpose
Feature: Injection Molding, PA66+MF40%, General PurposeApplication: Automotive (Engine Cover)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMID HI1202A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility
Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG ..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact
Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical LUMID SG2600B PA6+GF60%, General purpose, Good Surface
Feature: Injection Molding, PA6+GF60%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical Lupox® DP1000DU PBT
Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical Lupox® GP1000A PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical Lupox® GP2056F PBT+GF5%
Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical Lupox® GP2156FL PBT+GF15%
Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical Lupox® GP2306FC PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP2102 PC+GF10%
Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance
Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Molding
LG Chemical Lupox® SG5500 PBT+PET+GF50%
Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP1000MD PC, Light Diffusion
Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP1000MU PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C..
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP1006FL PC, Flame Retardant
Description: Injection Molding, PC, Flame Retardant, High FlowApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP1006FM PC, Flame Retardant
Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Lubrizol Estane® S385A Thermoplastic Polyurethane
Type: Estane® S385A is a Shore 85A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Information Provi..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Lubrizol Estane® T460A Thermoplastic Polyurethane
Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Lubrizol Estane® T470A Thermoplastic Polyurethane
Type: Estane® T470A is a Shore 77A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Lubrizol Estane® L194A Thermoplastic Polyurethane
Type: Estane® L194A is a Shore 95A, polyester grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: AsiaInformation Provided by The Lubrizol Corporation
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance
Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Copyright © lookpolymers.com All Rights Reserved