Taiwan Sheen Soon Sheenthane® A9315E Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® A9315E Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 91 - 95
91 - 95
Tensile Strength 49.0 MPa
7110 psi
Elongation at Break 400 %
400 %
100% Modulus 0.01273 GPa
1.846 ksi
300% Modulus 0.0294 GPa
4.27 ksi
Processing Properties Metric English Comments
Processing Temperature 180 - 210 °C
356 - 410 °F