Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP540S Injection Molding Grade Polypropylene Moplen EP540S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540S is a block copolymer particularly suitable for injection.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP640R Injection Molding Grade Polypropylene Moplen EP640R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640R is a block copolymer particularly suitable for injection.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP640S Injection Molding Grade Polypropylene Moplen EP640S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640S is a block copolymer particularly suitable for injection.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP640T Injection Molding Grade Polypropylene Moplen EP640T is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640T is a block copolymer suitable for injection molding of a.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP300H Injection Molding Grade Polypropylene Moplen EP300H is a heterophasic copolymer, suitable for injection moulding as well as for thermoforming applications. Moplen EP300H is a excellent low temperature impact behavior combined with a goo.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP301C Pipe Extrusion/ Sheet/ Blown Film Grade Polypropylene Moplen EP301C is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP301C is a block copolymer suitable for industrial pipe and se.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP540R Injection Molding Grade Polypropylene Moplen EP540R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540R is a block copolymer particularly suitable for injection.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP540T Injection Molding Grade Polypropylene Moplen EP540T is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540T is a block copolymer particularly suitable for injection.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
PolyMirae Moplen EP641P Injection Molding Grade Polypropylene Moplen EP641P is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP641P is a block copolymer suitable for injection molding of c.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene B240LP PP B240LP Extrusion Impact CopolymerApplications:Extrusion blow moldingCharacteristics:High impactHeat stabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene C600M2 PP C600M2 Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene J440 PP J440 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene J640 PP J640 Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene J640A PP J640A Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporatio.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene J640U PP J640U Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityWeatherabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene J740 PP J740 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporation.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene R530 PP R530 Random CopolymerApplications: EBMCharacteristics: Transparency USP Class VI certifiedInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Hyosung Topilene R530A PP R530A Random CopolymerApplications: ISBMCharacteristics: Transparency USP Class VI certifiedInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 27.5 MPa @Thickness 3.20 mm |
3980 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
Global F-7000 High Density Polyethylene Description-high quality is suitable for blown film @wide range of size & thickness Applications-large & small rolled film, shopping bag, merchant bag, disposal waste bagInformation provided by Glob.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
LG Chemical LUTENE-H ME2500 HDPE Description: LUTENE-H ME2500 is mainly intended for injection molding of bottle caps. It has good gas permeability characteristics and high toughness.Applications: Caps for beverage bottlesCAS No. 9.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC M1425 Polypropylene Impact Copolymer Features: SEETEC M1425 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1425 exhibits a very high stiffness and a good impact strength. SEETEC M1425 meets the FD.. |
|||
Tensile Strength, Yield | 27.4 MPa | 3980 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® H5234 High Density Polyethylene ApplicationsALATHON H 5234 is a high flow injection molding grade of resin designed for fast cycle and thin wall molding. It provides cold temperature impact resistance. Typical applications inclu.. |
|||
Tensile Strength, Yield | 27.5 MPa @Thickness 3.20 mm |
3980 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | ASTM D638 |
SCG Chemicals EL-Proâ„¢ P642J Polypropylene Injection Molding Key Characteristics:Good flowabilityExcellent stiffnessHigh impact strengthMechanical property balanceContains UV stabilizer and anti-static agentRecommended Applications:Industrial and household pr.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S168D Thermoplastic Polyurethane Type: Estane® S168D is a Shore 68D, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The.. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® S195A Thermoplastic Polyurethane Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Tensile Strength, Yield | 27.5 MPa | 3980 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® S395A Thermoplastic Polyurethane Type: Estane® S395A is a Shore 95A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availa.. |