Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® 11T85 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Adequate hardness, excellent mechanical properties and easy processing.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ISO 868
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ISO 527-2/5A/500
Elongation at Break 640 %
640 %
ISO 527-2/5A/500
50% Modulus 0.00500 GPa
0.725 ksi
ISO 527-2/5A/500
100% Modulus 0.00600 GPa
0.870 ksi
ISO 527-2/5A/500
300% Modulus 0.0100 GPa
1.45 ksi
ISO 527-2/5A/500
Tear Strength 90.0 kN/m
514 pli
ISO 34-1B
Abrasion 20
20
mm<sup>3</sup>; ISO 4649-a
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 210 °C
410 °F
Zone 1 195 °C
383 °F
Zone 2 200 °C
392 °F
Zone 3 210 °C
410 °F
Zone 4 210 °C
410 °F
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F