Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 3 = 410 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 210 - 220 °C
410 - 428 °F
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp..
Zone 3 210 - 220 °C
410 - 428 °F
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-..
Zone 3 210 °C
410 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound
PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,..
Zone 3 210 °C
410 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
Zone 3 210 °C
410 °F
Die
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
Zone 3 210 °C
410 °F
Die
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
Zone 3 210 - 230 °C
410 - 446 °F
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro..
Zone 3 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 3 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical LI970HF Co-Extrusion ASA
Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical
Zone 3 210 - 220 °C
410 - 428 °F
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar..
Zone 3 210 - 230 °C
410 - 446 °F
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..
Zone 3 210 °C
410 °F
Injection Molding
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 3 210 - 240 °C
410 - 464 °F
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
Zone 3 210 - 260 °C
410 - 500 °F
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC)
TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products ..
Zone 3 210 °C
410 °F
Extrusion
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
Zone 3 210 - 220 °C
410 - 428 °F
Injection
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane
Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by..
Zone 3 210 - 220 °C
410 - 428 °F
Injection
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 3 210 - 220 °C
410 - 428 °F
Injection
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
Zone 3 210 - 220 °C
410 - 428 °F
Injection
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane
Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr..
Zone 3 210 - 220 °C
410 - 428 °F
Injection
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 3 210 °C
410 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Zone 3 210 °C
410 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Zone 3 210 °C
410 °F
Blown Film Coextrusion
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Zone 3 210 °C
410 °F
Cast Film/Sheet Processing
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Zone 3 210 °C
410 °F
Blown Film Coextrusion
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Zone 3 210 °C
410 °F
Extrusion Coating
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Zone 3 210 - 230 °C
410 - 446 °F
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene
OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances ..
Zone 3 210 °C
410 °F
Extrusion
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Zone 3 210 °C
410 °F
Extrusion
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..