Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 4085 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ISO 37 |
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU Type : Pearlthane® 11T85 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Adequate hardness, excellent mechanical propert.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T85E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ISO 37 |
Huntsman AVALON® 85 AE Thermoplastic Polyurethane Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
DuPont Vamac® HVG Sample Compound Test compound is press cured for 5 minutes at 175°C and post cured for 4 hours at 175°C.Information provided by DuPont. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2185 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-7180 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8280 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | DIN 53504 |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ISO 37 |
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1485RV Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1685AD Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D638 |
ELASTO UK Dryflex® 400901S SBS Based Material, 90A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D638 |
ELASTO UK Dryflex® 500900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D638 |
ELASTO UK Dryflex® 660900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D638 |
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1585 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00600 GPa | 0.870 ksi | ISO 37 |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |